Heating Plant Sabac in Serbia suffered oxygen pitting corrosion on three boilers. After one heating season a 2 inch Merus Ring HCI left a protective magnetite film and no yellow coatings.

De uitdaging

The Serbian Heating Plant Sabac experienced pitting corrosion on three large boilers. Yellow coatings on the tube surfaces indicated oxygen corrosion creating craters, causing pipe deterioration and requiring frequent costly replacements.

De Merus-oplossing

Installation of a Merus Ring on the supply line of boiler number 1 as a trial to prevent limescale, corrosion, and oxygen/pitting corrosion.

→After one heating season, comparison showed no more yellow coatings on the treated boiler surfaces. The pipes developed a black film of magnetite, which acts as an anti-corrosion agent. Boilers 2 and 3 without treatment showed unchanged deterioration. The facility determined the ring was as effective as claimed and decided to purchase Merus rings for all three boilers.

Klaar om uw water op de fysische manier te behandelen?

Vertel ons over uw systeem. Wij adviseren de juiste Merus Ring en spreken, waar dat helpt, een gemeten proef af met resultaten voor en na.

Vraag een advies aan